STUDIES ON MODIFIED POLYPROPYLENE FIBERS, PROPERTIES OF FIBER SPUN FROM A POLYBLEND OF POLYPROPYLENE AND A COPOLYMER OF STYRENE AND 2, 2, 6, 6-TETRA-METHYL-4-PIPERIDINYLMETHACRYLATE
返回论文页
Research Article|更新时间:2021-03-19
|
STUDIES ON MODIFIED POLYPROPYLENE FIBERS, PROPERTIES OF FIBER SPUN FROM A POLYBLEND OF POLYPROPYLENE AND A COPOLYMER OF STYRENE AND 2, 2, 6, 6-TETRA-METHYL-4-PIPERIDINYLMETHACRYLATE
Lu Qi-hao, Zheng Guo-xiu, Liang Wen-zhong, FENG Han-bao, Sun Euo-na, Hou Xiao-huai, Zhou Xiang-feng, Su Bing-lu, ZHAO Rui-nian, Shen De-kang. STUDIES ON MODIFIED POLYPROPYLENE FIBERS, PROPERTIES OF FIBER SPUN FROM A POLYBLEND OF POLYPROPYLENE AND A COPOLYMER OF STYRENE AND 2, 2, 6, 6-TETRA-METHYL-4-PIPERIDINYLMETHACRYLATE. [J]. Acta Polymerica Sinica (5):285-290(1979)
DOI:
Lu Qi-hao, Zheng Guo-xiu, Liang Wen-zhong, FENG Han-bao, Sun Euo-na, Hou Xiao-huai, Zhou Xiang-feng, Su Bing-lu, ZHAO Rui-nian, Shen De-kang. STUDIES ON MODIFIED POLYPROPYLENE FIBERS, PROPERTIES OF FIBER SPUN FROM A POLYBLEND OF POLYPROPYLENE AND A COPOLYMER OF STYRENE AND 2, 2, 6, 6-TETRA-METHYL-4-PIPERIDINYLMETHACRYLATE. [J]. Acta Polymerica Sinica (5):285-290(1979)DOI:
STUDIES ON MODIFIED POLYPROPYLENE FIBERS, PROPERTIES OF FIBER SPUN FROM A POLYBLEND OF POLYPROPYLENE AND A COPOLYMER OF STYRENE AND 2, 2, 6, 6-TETRA-METHYL-4-PIPERIDINYLMETHACRYLATE
6-Tetramethyl-4-piperidinylmethacrylate was prepared by ester-exchange reaction between 2
2
6
6-tetramethyl-4-piperidinol and methylmethacrylate. The resulting ester was copolymerized with styrene
and the copolymer was blended with polypropylene in quantities of 1.5-5%. The polyblends thus obtained were spun into fibers with a tenacity of about 4g/d. The modified fibers have a good resistance to weathering
and good dyeing ability with azo-type dispersive dyes. At the same time the spinning temperature of the polyblends was lowered to around 280℃.