Synthesis of HTPB with High cis-1,4 Content from PBD Original Solution
The original solution of polybutadiene (PBD) rubber from industrial plant was directly used as a starting material to synthesize hydroxyl-terminated polybutadiene (HTPB) with high cis-1
4 content and extremely low glass transition temperature for the first time.The synthetic process was divided into two parts
including the oxidolysis for the preparation of aldehyde group-terminated polybutadiene (ATPB) and the subsequent reduction reaction from ATPB to HTPB by NaBH4.The microstructure of PBD rubber nearly kept unchanged during the whole process so that the resulting HTPB retained a high cis-1
4 content ( 95%).The molecular weight was manipulated in the range of 2200~7000 (determined by 1H-NMR) by controlling the stoichiometric ratio between oxidant (mCPBA) and butadiene units with the polydispersity index within 1.5~2.1
and the functionality (fn) of HTPB was close to 2.0.In comparison with the HTPB prepared by the anionic or free radical polymerization
the HTPB with high cis-1
4 content possesses more regular microstructure (cis-1
4 95%) and extremely low glass transition temperature (Tg -104 ℃).Meanwhile
many high energy-cost and time-consuming processes
such as steam agglomeration and drying in PBD rubber production
and cutting
swelling and dissolving of slab rubber during the preparation of HTPB
can be removed.In short
this process was more economic
efficient and controllable.